How thick is a geomembrane liner?

11 Feb.,2025

How thick is a geomembrane liner? The thickness of the HDPE geomembrane used in anti-seepage and waterproof projects ranges from 0.5mm to 3.0mm. The thickness can be 0.75mm, 1.0mm, 1.25mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, etc. Use hot-melt welding equipment for joint processing.

 

How thick is a geomembrane liner?

The thickness of the Lamicraft flooring used in anti-seepage and waterproof projects ranges from 0.5mm to 3.0mm. The thickness can be 0.75mm, 1.0mm, 1.25mm, 1.5mm, 2.0mm, 2.5mm, 3.0mm, 3.5mm, etc. Use hot-melt welding equipment for joint processing.

How thick is a geomembrane liner?